이배훈님의 답변
2014-04-02- 0
문헌에서 NMP와 acetone을 사용하네요. (polar한 solvent 사용)
In the second process, ZnO (Inframat Advanced Materials, average particle size: ~30nm) and PVDF (Alfa Aesar, m.p.155 -160°C) are utilized as powders. Through this method, nanocomposite of %65 volumetric ZnO loading are produced. Ceramic/polymer composites are prepared by first dissolving PVDF in hot acetone, placing ceramic
nanopowder into this solution and mixing it for 5 minutes via a POLYTRON PT600 type benchtop homogenizer. After nitrogen gas is introduced to remove acetone until a gel-like soft paste is obtained, this paste is pressed into wet pellets
using a Specac pellet press at a pressure of about 2000 psi.
PVDF is the standard binder material used in the production of composite electrodes for lithium ion batteries. 1-2% weight solution of PVDF dissolved in N-methyl-2-pyrrolidone (NMP) is mixed with an active lithium storage material such as graphite, silicon, tin, LiCoO2, LiMn2O4, or LiFePO4 and a conductive additive such as carbon black or carbon nanofibers. This slurry is cast onto a metallic current collector and the NMP is evaporated to form a composite or paste electrode. PVDF is used because it is chemically inert over the potential range used and does not react with the electrolyte or lithium.- wiki pedia- -
답변
조윤환님의 답변
2014-04-03- 0
반갑습니다.
ZnO는 세라믹이고 PVDF는 고분자 물질이므로 두 물질을 모두 녹여서 혼합할 계획은 아닐 것으로 생각합니다. 즉 PVDF만 녹일 수 있으면 될 것입니다.
PVDF는 다른 용매에 비해 polar aprotic solvent에 용해도가 상대적으로 높은 편입니다. 절대적인 기준이 아니라 상대적 기준임을 명심하시길...
NMP, DMSO, DMF, DMAC, acetonitrile 등이 적합한 용매 입니다. acetone과 ethyl acetate에도 녹기는 하지만 그 양이 매우 적습니다.
다음은 3M사가 제공하는 PVDF 기술문서 입니다. 내화학성에 대해 자세한 표가 첨부되어 있으니 참고하시기 바랍니다.
http://multimedia.3m.com/mws/mediawebserver?mwsId=66666UF6EVsSyXTt4xTV4xT2EVtQEVs6EVs6EVs6E666666--&fn=98-0504-1514-4.pdf